PA66 Granules Moisture Control: Drying vs Conditioning in a Moulding Trial

Drying PA66 granules before moulding and conditioning a moulded PA66 part afterwards are two different controls. The first concerns the feedstock entering the machine. The second defines the state in which the finished part is measured and tested. A useful trial record identifies both states, the exact proposed grade and the time of each inspection. Otherwise, two suppliers may appear to offer different results simply because their samples were prepared and measured differently.

This guide focuses on the moisture record. For the wider drawing, service and sourcing brief, see our PA66 granules buyer guide and existing PA66 granules page.

Before moulding: identify the grade and its handling instructions

Start with the proposed grade designation and its current technical data sheet and processing instructions. Ask the supplier which storage, drying and moisture-check procedure applies to that grade. PA66 is a polymer family, not one universal drying recipe. Reinforcement, additives, colour and packaging can differ between candidate compounds.

For the material issued to the trial, record:

  • Supplier grade designation, batch or lot, and package identification.
  • Whether the package was sealed, damaged or previously opened, plus the opening time.
  • The drying equipment and the settings actually used, including duration and any interruption.
  • The moisture measurement method and result, if your processor measures it, and the time between drying and feeding.

Do not copy a temperature or time from a different manufacturer's grade into a Haishengda trial. BASF's Ultramid processing guidance explains that excess moisture can affect moulded-part quality and that detailed processing recommendations are grade-specific. Its published values describe BASF products, not a specification or performance claim for Haishengda material.

During moulding: keep the material record with the part record

Use one trial sheet for the candidate grade, machine, mould revision and material preparation. Record the settings chosen by the processor from the proposed grade's instructions, then note any changes made during the run. Label samples with the lot and run number so that a later appearance or dimensional result can be traced to the conditions that produced it.

Compare like with like. If supplier A's parts were made from a freshly opened package and supplier B's parts from an opened package that was re-dried, write that difference down before interpreting the result. If a run is interrupted, record when material remained in the feed system and how the restart was handled. The aim is a repeatable comparison, not a claim that one condition automatically makes every PA66 grade suitable.

After moulding: define the inspection condition

Agree which measurements are taken immediately after moulding and which are taken after a specified storage or conditioning period. Mark the drawing features that matter for assembly: for example, a locating face, clip, hole spacing or insert position. Record the inspection date and the condition of the specimen next to each result.

Polyamide properties and dimensions can change as a moulded part takes up moisture. BASF's Ultramid product brochure discusses conditioning and shows why the time to reach a condition depends on part thickness. A BASF PA66 grade page separately identifies dry-as-moulded and conditioned values. These sources illustrate the need to label the test state; they do not establish the properties of a different supplier's grade.

For each candidate, use the same agreed conditioning method and inspection schedule. If your customer specifies a test condition, use that requirement. If it does not, ask engineering to define one before treating small differences between samples as material differences. Keep initial and conditioned results in separate columns instead of mixing them into a single pass/fail line.

A short acceptance record

Before the trial, write down who approves each check and what counts as a pass. Include the drawing revision, critical dimensions and tolerances, appearance criteria, assembly fit and any application-specific tests. Record the sample count and test method. A change in grade, material preparation or conditioning calls for a new, traceable result rather than reusing the previous approval.

Is drying PA66 granules the same as conditioning a PA66 part?

No. Drying prepares the granules for processing; conditioning defines the post-moulding specimen state for inspection or use. Record both independently.

Can two PA66 sample results be compared if one was measured dry and the other conditioned?

Not as a direct material comparison. First align the grade-specific preparation, part geometry, measurement method and agreed specimen condition, or label the difference explicitly.

What should I send to discuss a PA66 moulding trial?

Send the drawing, current or candidate grade, critical dimensions, service conditions, production method, trial quantity and the required inspection condition. Ask for the proposed grade's own processing and documentation package.

Use the Haishengda contact form or WhatsApp to send the project brief. Material selection and final-part approval remain subject to the proposed grade's documents and your own tests.

Send your material requirements

Scroll to Top